Hi guys, just to add some more info, I received my rebodied Zenton b42, about 2 weeks ago, and according to Zenton it uses AB5S (CuAl11Fe6Ni6), sourced from Germany. It cefrtainly is a huge difference from the brass case, it has a nice even patina, I've been on vacation at the beach so it has had hours upon hours of exposure to salt water day after day for the last two weeks, looks great. I'll try to post some pics of it as soon as I can .