View single post by Amer.S | |||||||||||||
Posted: Thu Sep 29th, 2011 03:13 pm |
|
||||||||||||
Amer.S![]()
![]() |
Heya Stew, It is for sure not going fast....Perhaps the temps.....Mine start hot/warm when dunked....It could also be the ratio of mix, 2 teaspoons gel/12 oz of water. (Plus to be honest I have no idea how long the stuff was sitting on the shelf prior to shipping...Could be a small factor) Also yours is UNI VS. the second gen is CU....Not sure if the properties react differently to the mix of sulfur...Look at the silver bracelet in Steve's pix or the youtube video https://www.cooltools.us/Cool-Tools-Liver-of-Sulfur-in-Gel-Form-p/pol-800parent.htm?1=1&CartID=0 Color changed pretty quick..I also wonder if density/mass has anything to do with it even though the outer layer is what patina's I am not a metal specialist nor chemist so my points above could mean nothing....I honestly prefer the natural way...hence what I did with the 2 Nimo's so this is a fun experiment for me...Ultimately no rush on my part. /Amer
|
||||||||||||
|